MEMSnet Home: MEMS-Talk: Is there any way I can deposit gold onto pyrex wafer directly?
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-22
sokwon Paik
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-23
Gautham V
Is there any way I can deposit gold onto pyrex wafer directly?
2003-04-23
transene
Is there any way I can deposit gold onto pyrex wafer directly?
Gautham V
2003-04-23
Hi Paik,
I used sputter process on Pyrex for my evaluations. Direct gold has good
initial adhesion. Once you try to increase the thickness it results in poor
adhesion. You need to do a lot of surface treatment on the Pyrex to get a
good adhesion. Try a layer of Ti (1000A) and then gold. This will help.
Platinum sputter target exists. Price depends on the target size. Check with
BPS and other material suppliers.
Regards Gautham. V

----- Original Message -----
From: "sokwon Paik" 
To: 
Sent: Wednesday, April 23, 2003 12:37 AM
Subject: [mems-talk] Is there any way I can deposit gold onto pyrex wafer
directly?


> I'm a student of Texas A&M University.
> As far as I know, gold doesn't attach to pyrex glass
> directly. But I think if I use sputtering machine then
> it might be possible.
> Anybody tried to attach gold directly onto pyrex
> wafer?
> One more question. Is there platinum sputtering source
> exist?
> If so, how much is it? Please answer me the question.
> I appreciate your any reply.
> Thanks,
>
> sokwon Paik
>
>
> __________________________________________________
> Do you Yahoo!?
> The New Yahoo! Search - Faster. Easier. Bingo
> http://search.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
The Branford Group
Nano-Master, Inc.