off-axis wafer etching
2003-04-23
li zhiping
2003-04-23
David Nemeth
2003-04-24
transene
off-axis wafer etching
li zhiping
2003-04-23
Hi,
I want to ask a question. If I make a protecting pattern, say by LTO,on a
weird wafer surface, which has a 9 degree to <100>, and put it in KOH or
TMAH for tens minutes, Could the wafer be etched to the <100> at the
unprotected area? Thanks!
Zhiping





_________________________________________________________________
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.