MEMSnet Home: MEMS-Talk: Fix Fibre in Groove
Fix Fibre in Groove
2003-04-23
Jun yao
2003-04-23
Jing Liu
2003-04-24
transene (2 parts)
Photoresist
2003-04-24
krishna
Fix Fibre in Groove
Jun yao
2003-04-23
Now, I am working on a structure that is used to switch a single mode fibre, and
I encountered a problem which should be easy for an experienced MEMS researcher.



My question is how to fix the fibre in the groove? Using some kind of glue? the
problem is that if the dimension of the groove is large, it is simple to put the
glue, hoever, the groove structure can not be released (takes a very long time
to do this), and if it is small, the structure will be fixed as well (stick to
the substrate) when the glue is used.



If you have an idea about this problem, please send me email. Thank you!



Sincerely yours,



Jun Yao



---------------------------------
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer