Dear members,

I am looking for a supplier who can supply positive
photoresist that is suitable for gold electroplating.

The plating bath i am using is of cyanide type and i
am looking for the photoresist that can resist cyanide
attack.


Thanks

Kris


__________________________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo
http://search.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing