Kris,
     As an alternative you may want to think metal lift off.  Using image
reversal 800 angstrom lines and spaces are possible. Also 40 micron thick resist
for thick, 20 angstrom metal plate up or lift off, is easy.  let me know if you
need details.  Bill Moffat

-----Original Message-----
From: krishna [mailto:[email protected]]
Sent: Wednesday, April 23, 2003 11:03 PM
To: General MEMS discussion
Subject: [mems-talk] Photoresist


Dear members,

I am looking for a supplier who can supply positive
photoresist that is suitable for gold electroplating.

The plating bath i am using is of cyanide type and i
am looking for the photoresist that can resist cyanide
attack.


Thanks

Kris


__________________________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo
http://search.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.