looking for wafer supplier
Mario Robles
2003-04-24
Hello,

You can try contacting Silicon Quest at 408-496-1000 and speak with
Yvonne. If they can not help then she may be able to direct you to
another company.

Thank you,

Mario Robles

Tanaka Systems, Inc.
2577 Leghorn Street
Mountain View, CA 94043

650-966-8001 ofc
650-966-1881 fax
www.dicingblades.com 

DICING BLADES * BACKGRIND WHEELS * DICING PROCESS DEVELOPMENT

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Yilei
Sent: Wednesday, April 23, 2003 10:01 AM
To: [email protected]; [email protected]
Subject: [mems-talk] looking for wafer supplier

Hi Member:
I need some wafers with following structure to do my research project,
from
bottom to top: silicon dioxide, silicon, silicon dioxide, polysilicon.
We only
have special requirements to the polysilicon layer, for example, grain
size,
crystalline, etc.

Can anyone help me where I can find them? If possible, the cost and the
choices
we have for the polysilicon layer. Now we only need a small batch and
maybe a
little more later.

Thanks and regards,
Yilei




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
MEMS Technology Review
Nano-Master, Inc.