Fix Fibre in Groove
2003-04-23
Jun yao
2003-04-23
Jing Liu
2003-04-24
transene (2 parts)
Photoresist
2003-04-24
krishna
Fix Fibre in Groove
transene
2003-04-24
Transene Company offers a range of epoxy adhesives which may perform
well in this application.  These products may be viewed at
www.transene.com by choosing Catalogs and the Epoxy Adhesives menu
option.

Christopher Christuk
Transene Company
Tel:  978 777 7860
Email:  [email protected]

-----Original Message-----
From: Jing Liu [mailto:[email protected]]
Sent: Wednesday, April 23, 2003 1:06 PM
To: Jun yao
Cc: [email protected]
Subject: Re: [mems-talk] Fix Fibre in Groove

You may like to try high viscosity epoxy and use probe to put it between
your fiber and structure.

Jing Liu


On Wed, 23 Apr 2003, Jun yao wrote:

>
> Now, I am working on a structure that is used to switch a single mode
fibre, and I encountered a problem which should be easy for an
experienced MEMS researcher.
>
>
>
> My question is how to fix the fibre in the groove? Using some kind of
glue? the problem is that if the dimension of the groove is large, it is
simple to put the glue, hoever, the groove structure can not be released
(takes a very long time to do this), and if it is small, the structure
will be fixed as well (stick to the substrate) when the glue is used.
>
>
>
> If you have an idea about this problem, please send me email. Thank
you!
>
>
>
> Sincerely yours,
>
>
>
> Jun Yao
>
>
>
> ---------------------------------
> Do you Yahoo!?
> The New Yahoo! Search - Faster. Easier. Bingo.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


EPOXY.DOC (application/msword, 167936 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering
Nano-Master, Inc.