Neal Ricks
Gray Scale Masks
Neal Ricks
2003-04-24
Han, I disagree with Vic's assessment since gray scale mask making is not solely
an issue of being able to vary the binary optical density with patterning.  The
actual glass is very special as well, and I believe proprietary.  That is why I
refered you to Canyon. Neal Neal RicksWafer Fab ManagerShipley Co., LLCEIF Div.
- Opto Group

[email protected] wrote:Han,

I service equipment for a photomask shop called IC Photomask. They're located
in Chandler, AZ. They recently did a mask that had 270 million, 2.5 micron
opaque circles in a 4"x4" area of a 5"x5" plate. So I think gray scale masks
should be no problem for them. Their number is 480-892-2420

Best Regards,

Vic




Hi all,
>
> Does any one know where can I get a gray scale mask to be made?
>
> Thanks
>
> regards
>
> Han
>
> RMIT University

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


---------------------------------
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Harrick Plasma, Inc.
Addison Engineering