Silicon Etch Rates for Various Etchants
nga
2003-04-28
You can find some information on Silicon sensor and circuits: onc chip
compatibility" in chapter 2
Edited by R.F.Wolffenbuttel, Chapmal Hall 1996


At 11:42 AM 4/26/03 -0500, you wrote:
>Hi,
>Does anyone know a good source (book, review article, etc.) for the
>silicon etch anisotropies (Si(111) versus Si(100)) and oxide etch
>selectivities of KOH, EDP, TMAH, Hydrazine, and related etchants?
>Thanks in advance,
>
>Preston Larson
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group