MEMSnet Home: MEMS-Talk: Silicon Etch Rates for Various Etchants
Silicon Etch Rates for Various Etchants
2003-04-26
preston
2003-04-28
nga
2003-04-28
Andreas Jahn
2003-04-28
Kirt & Erika Zipf-Williams
2003-04-28
[email protected]
Silicon Etch Rates for Various Etchants
Andreas Jahn
2003-04-28
Hi Preston,

for TMAH check this paper out: "Dual-doped TMAH silicon etchant for
microelectromechanical structures and systems application".

-Andreas

-----Original Message-----
From: preston [mailto:[email protected]]
Sent: Saturday, April 26, 2003 12:43 PM
To: [email protected]
Subject: [mems-talk] Silicon Etch Rates for Various Etchants


Hi,
Does anyone know a good source (book, review article, etc.) for the
silicon etch anisotropies (Si(111) versus Si(100)) and oxide etch
selectivities of KOH, EDP, TMAH, Hydrazine, and related etchants?
Thanks in advance,

Preston Larson




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review