Silicon Etch Rates for Various Etchants
Kirt & Erika Zipf-Williams
2003-04-28
See the book Properties of Crystalline Silicon (a thick yellow book), edited
by Robert Hull, published by IEE/INSPEC in 1999.
Chapter 16, entitled "Etching of Single-Crystal Silicon,"
has a large review with etch rates for different solutions (including those
below), crystal directions, etc., with references.
        --Kirt Williams, Ph.D.   consultant

----- Original Message -----
From: preston 
To: 
Sent: Saturday, April 26, 2003 9:42 AM
Subject: [mems-talk] Silicon Etch Rates for Various Etchants


> Hi,
> Does anyone know a good source (book, review article, etc.) for the
> silicon etch anisotropies (Si(111) versus Si(100)) and oxide etch
> selectivities of KOH, EDP, TMAH, Hydrazine, and related etchants?
> Thanks in advance,
>
> Preston Larson
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group