MEMSnet Home: MEMS-Talk: Au etchant
Au etchant
2003-04-30
Sang Hwui Lee
2003-04-30
Mighty Platypus
2003-04-30
Kirt & Erika Zipf-Williams
equipment
2003-04-30
RobDavis
2003-05-01
Roger Shile
2003-04-30
Rojano, Gabriel
Au etchant
Mighty Platypus
2003-04-30
Transene makes one called TFA that is pretty good. It takes less than 20
seconds for it to etch 1000A of Au, and I had no problems with it.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Observations of nature, no matter how seemingly arcane, are like
peeling off one more layer from the great onion of knowledge"
    -- Don Petit, ISS science officer

On Wed, 30 Apr 2003, Sang Hwui Lee wrote:

> Hello,
>
> Does anyone know the recipe of Au etchant or the product name for Au
> etchant? I have Au/Cr deposited pyrex glass wafer. now I don't have Au
> etchant. Au etchant should not attack Cr layer or interface of Cr/glass
> since Au/Cr would be window for glass isotropic etching in BOE.
>
> thanks,
>
> SangHwui Lee
> Ph.D candidate/MSE/NJIT
> Microelectronics Research Center(MRC)
> 973-596-6368(O)
> 201-242-1486(H)
>
>
>
>
>
> _________________________________________________________________
> MSN 8 helps eliminate e-mail viruses. Get 2 months FREE*.
> http://join.msn.com/?page=features/virus
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Nano-Master, Inc.
MEMStaff Inc.