Phillipe Tabada
tooling for HF release etch
Phillipe Tabada
2003-04-30
Hi Robert,

     Another solution a collegue of mine used was to cut out the flat
circular portion of a teflon petri dish and buy yourself teflon screws and
nuts which can be used to hold your die in place.  This way you can have a
holder suitable for the desired die size and is compatible with HF.  Just
make sure the holder you make goes through a full RCA clean to remove any
contamination.

Phil Tabada


>From: "Kirt & Erika Zipf-Williams" 
>Reply-To: General MEMS discussion 
>To: "General MEMS discussion" 
>Subject: Re: [mems-talk] tooling for HF release etch
>Date: Tue, 29 Apr 2003 11:06:43 -0700
>
>An alternative is to place the dice on a Gel-Pak insert for etching.
>The dice stick pretty well in HF.
>     --Kirt Williams, Ph.D.   consultant
>
>----- Original Message -----
>From: Robert Dean 
>To: General MEMS discussion 
>Sent: Monday, April 28, 2003 5:36 PM
>Subject: [mems-talk] tooling for HF release etch
>
>
> >
> > >Hello,
> >
> > I am looking for a ladle-like tool or small "bucket" for transferring
>die
> > to and from, and to hold them in a beaker of HF for a standard SOI MEMS
> > process release etch.  Any suggestions on what and where to purchase it?
> >
> > Sincerely,
> >
> > Robert Dean
> >
> >
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/


_________________________________________________________________
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Addison Engineering