Dear colleagues,

I'm going to use some ultra thin silicon wafers (10-20um). I found meet a
basic problem----how can I handle them without making it broken. Any
suggestion would be appreciated.

Hongjun Zeng
**********************************************
Microfabrication Applications Laboratory (MAL)
University of Illinois at Chicago
ERF Building, 842 W. Taylor Street
Chicago, IL 60607-7022
Tel.: 312-413-5889, Fax: 312-996-6465
**********************************************



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.