MEMSnet Home: MEMS-Talk: How to handle ultra thin wafer
How to handle ultra thin wafer
2003-05-01
Hongjun Zeng
2003-05-02
Luesebrink Helge
How to handle ultra thin wafer
Luesebrink Helge
2003-05-02
Dear Hongjun,

Check out http://www.evgroup.com/products/tempbonder.htm

For temporary bonding your substrate to a carrier and release after the process
is done. On the Web site you will find papers and application notes on temporary
bonding and debonding as well.

Best regards,
Helge

-----Original Message-----
From: Hongjun Zeng [mailto:[email protected]]
Sent: Thursday, May 01, 2003 4:17 PM
To: MEMS2
Subject: [mems-talk] How to handle ultra thin wafer


Dear colleagues,

I'm going to use some ultra thin silicon wafers (10-20um). I found meet a
basic problem----how can I handle them without making it broken. Any
suggestion would be appreciated.

Hongjun Zeng
**********************************************
Microfabrication Applications Laboratory (MAL)
University of Illinois at Chicago
ERF Building, 842 W. Taylor Street
Chicago, IL 60607-7022
Tel.: 312-413-5889, Fax: 312-996-6465
**********************************************



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics