MEMSnet Home: MEMS-Talk: Borosilicate Glass Holes
Borosilicate Glass Holes
2003-05-02
B Swope
2003-05-02
Jon Hiller
2003-05-02
Henry Helvajian
Borosilicate Glass Holes
Jon Hiller
2003-05-02
Try using a Focused Ion Beam (FIB).

Jon

Jon M. Hiller
Electron Microscopy Center
Argonne National Laboratory
9700 South Cass Avenue
Argonne, IL.  60439
Tel:  630-252-9558
Fax:  630-252-4289


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of B Swope
Sent: Friday, May 02, 2003 09:53
To: [email protected]
Subject: [mems-talk] Borosilicate Glass Holes

Hello,
I was wondering if anyone has any success with creating small ( <50
microns) holes in borosilicate glass.  I am currently using an ablation
laser with mixed results...Any advice or suggestions would be greatly
appreciated.
Thanks,
Brett Swope

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering
The Branford Group