Carmen
2003-05-07
Hi all,

    I would like to know whether someone who have tried to deposit Cr
and Au by using sputter and then etched them successfully. I faced the
problem that the Cr layer cannot be etched completely after etching the
Au layer, and the color of the Cr layer is not silver, it is like green.
Is there any reason to cause the Cr layer become green if I use sputter
to deposit it? Do you have any idea for what the green layer is? (Is it
a compound or oxide).
Thank you very much.

Best Regards,
Carmen



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
MEMS Technology Review
Mentor Graphics Corporation