MEMSnet Home: MEMS-Talk: Cr and Au deposition by using sputter
Cr and Au deposition by using sputter
2003-05-07
Carmen
2003-05-07
R. Brent Garber (2 parts)
2003-05-07
Rodger Cary
2003-05-07
[email protected]
2003-05-08
leonid bikov
Cr and Au deposition by using sputter
leonid bikov
2003-05-08
Hi, Carmen,
Do your wafers see temperature above 250C after sputtering?
Interdiffusion of Cr to Au at temperatures above 250C is well known
problem and this may cause the problems with etching.

Best regards,

Leonid

-----Original Message-----
From: Carmen [mailto:[email protected]]
Sent: Wednesday, May 07, 2003 4:02 PM
To: [email protected]
Subject: [mems-talk] Cr and Au deposition by using sputter


Hi all,

    I would like to know whether someone who have tried to deposit Cr
and Au by using sputter and then etched them successfully. I faced the
problem that the Cr layer cannot be etched completely after etching the
Au layer, and the color of the Cr layer is not silver, it is like green.
Is there any reason to cause the Cr layer become green if I use sputter
to deposit it? Do you have any idea for what the green layer is? (Is it
a compound or oxide). Thank you very much.

Best Regards,
Carmen



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Addison Engineering
Nano-Master, Inc.