Hi all,

I was doing gold electroplating using cynide bath.I
was doing plating on Si wafer sputtered with gold
later covered with photoresist ,exposed and developed
and hardbaked.

after doing the above i have tried AU electroplating.I
was  going for very low current densities and very low
temperature and with optimum PH after very less time i
could obsevere the plating of gold but the Photoresist
is disturbed and the pattern was disturbed.

Can i find any ways to improve adhesion of photoresist
on AU surface.

Ur suggestions are highly appreciated.

Thanks
Kris


__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
University Wafer