MEMSnet Home: MEMS-Talk: Thin Membrane etching
Thin Membrane etching
2003-05-08
Sriram Akella
2003-05-09
Tobias Kramer
2003-05-08
Mark Fuller
2003-05-09
Burkhard Volland
2003-05-09
David Springer
Thin Membrane etching
Burkhard Volland
2003-05-09
Hello.


>Hi Everyone,
>
>   I am trying to etch 2 micron thick membrane. I am
>using TMAH as the etchant, but the etchrate of TMAH
>maintained at 80C is varying a lot.


Are you using an etch-stop technique?
Is the main problem the reproducibility of membrane thickness? Thickness
homogenity across the wafer?

> Can anyone suggest a procedure that is reproduce able
>to a fairly large extent.

I assume the membrane is made of silicon. You can use an electrochemical
etch stop. This will stop the etching at about the depth of the
implantation, depending on stopping voltage.
Or use SOI wafers, with 2 um device layer. Etch the handle wafer, and use
the oxide layer as etch stop.

Regards

Burkhard



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering