Sriram Akella
2003-05-09
Tobias Kramer
2003-05-08
Mark Fuller
2003-05-09
Burkhard Volland
2003-05-09
David Springer
Thin Membrane etching
David Springer
2003-05-09
Sriram.

Can you give us a few more details. What is the membrane made of and what are
the steps you are using to make it.

Thanks
David Springer


 >>  Hi Everyone,

 >>  I am trying to etch 2 micron thick membrane. I am
 >>  using TMAH as the etchant, but the etchrate of TMAH
 >>  maintained at 80C is varying a lot.

 >>  Can anyone suggest a procedure that is reproduce able
 >>  to a fairly large extent.

 >>  regards,
 >>  sriram

 >>  _______________________________________________
 >>  [email protected] mailing list: to unsubscribe or change your list
 >>  options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
 >>  Hosted by the MEMS Exchange, providers of MEMS processing services.
 >>  Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering