MEMSnet Home: MEMS-Talk: Photoresist for AU plating
Photoresist for AU plating
2003-05-09
Greg Miller
Photoresist for AU plating
Greg Miller
2003-05-09
Kris,

AP100 is an adhesion promoter for gold http://www.siliconresources.com/

Good Luck,

Greg Miller
KVH

-----Original Message-----
From: krishna [mailto:[email protected]]
Sent: Thursday, May 08, 2003 9:09 PM
To: General MEMS discussion
Subject: [mems-talk] Photoresist for AU plating


Hi all,

I was doing gold electroplating using cynide bath.I
was doing plating on Si wafer sputtered with gold
later covered with photoresist ,exposed and developed
and hardbaked.

after doing the above i have tried AU electroplating.I
was  going for very low current densities and very low
temperature and with optimum PH after very less time i
could obsevere the plating of gold but the Photoresist
is disturbed and the pattern was disturbed.

Can i find any ways to improve adhesion of photoresist
on AU surface.

Ur suggestions are highly appreciated.

Thanks
Kris


__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review
Addison Engineering