dear colleagues
     I have been working on a PECVD SiN 2000A dielectric directly on Au layer
(In a new STS PECVD equip.capactive coupled plasma, 8" plates,temperature 300
centidegree ).However the film is full of uniformly scattered black dots 1
micron or less (film extrusion under SEM )in diameter. No such dots found on SiN
on Silicon surface. Can anyone give me some explain and/or improvement advise.
BTW,Need I deposite oxide before SiN deposition? can you give me a good way to
pattern the SiN without affecting the Au/Cr beneath? ThX in advance.



        致
礼!


        miaomin
        [email protected]
          2005-05-13



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
The Branford Group
Nano-Master, Inc.