Jim,
    Is the HMDS prime vacuum vapor prime.  The vacuum dehydration removes
moisture, HMDS reacts with moisture leaving molecular sights that can lift
causing poor adhesion.  Bill Moffat

-----Original Message-----
From: Jim Beall [mailto:[email protected]]
Sent: Tuesday, May 13, 2003 1:50 PM
To: [email protected]
Subject: [mems-talk] photoresist adhesion to Tungsten


Dear All -

A colleague is using photoresist and a hydrogen peroxide wet etch to
pattern 200 nm thick W films. He is having adhesion problems for
etches longer than 30 seconds (large areas of PR peel off). He has
tried HMDS prime, 120 C post bake, etc. The post bake helped a
little, but he needs a more durable coat.

Does anyone have any lore for increasing PR adhesion to W in  a
hydrogen eroxide etch?

Thanks,

Jim
--

  - Jim Beall 303-497-5989
    [email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review