A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Etching SiO2 without affecting Aluminum
Etching SiO2 without affecting Aluminum
2003-05-15
bobo
2003-05-15
Tobias Kramer
2003-05-15
beaton@npphotonics (Bill Eaton)
2003-05-15
Kirt & Erika Zipf-Williams
2003-05-15
Mark McNie
2003-05-16
Neal Ricks
2003-05-15
Pavel Neuzil
2003-05-15
Dave Kharas
2003-05-16
[email protected]
2003-05-16
David Springer
Etching SiO2 without affecting Aluminum
Kirt & Erika Zipf-Williams
2003-05-15
Use Pad Etch 4 from Ashland.
It is formulated to etch through oxide and barely etch underlying aluminum.

    --Kirt Williams, Ph.D.    consultant

----- Original Message -----
From: bobo 
To: 
Sent: Wednesday, May 14, 2003 9:30 PM
Subject: [mems-talk] Etching SiO2 without affecting Aluminum


> Dear all,
> does anyone knows what wet etchant can etching silicon dioxide without
etching aluminum at the same time?   Thanks.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics