vapor phase anti-stiction coatings
2003-05-16
Dave Kharas
2003-05-16
Madanagopal K.V.
2003-05-27
Bill Moffat
vapor phase anti-stiction coatings
Madanagopal K.V.
2003-05-16
Parylene might be an option:  http://www.scscookson.com/applications/mems.cfm

Madan.

At 08:15 AM 5/16/2003 -0700, you wrote:
>Dave Kharas 

___________________________________________________________

K.V.Madanagopal, Ph.D.
Senior Research Associate
Alliance for Nanomedical Technologies
311 Stocking Hall
Cornell University
Ithaca
NY 14850
Fax:607-255-8741
Phone:607-254-8052
___________________________________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
University Wafer