Hi folks,
I wonder if anyone knows about the strain of SiO2 and
SixNy on Ge. I tried LTO oxide (450oC), but it seems
that there is tensile strain in oxide layer. I want to
find film with no strain or a little bit compressive.
Any info is appreciated.
Thanks.
Song


__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
MEMS Technology Review
Mentor Graphics Corporation