MEMSnet Home: MEMS-Talk: boron implant
boron implant
2003-05-21
Ravi Shankar
2003-05-22
[email protected]
boron implant
[email protected]
2003-05-22
Are you doing the ion implantation? Could you tell me what
is the kinetic energy and dose in your process?

> Hi
> i was trying to implant boron through 1000A SiO2. After
> annealing the wafer, we tried to strip the SiO2 in HF and
> BOE. The sample dewetted in HF failed to give any sheet
> resistance value in four probe measurement, whereas one
> done in BOE gave the reading. can anyone suggest the
> reason behind it.
> Ravi Shankar
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or
> change your list options, visit
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing
> services. Visit us at http://www.memsnet.org/

Best Regards,
Kin


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering