MEMSnet Home: MEMS-Talk: etch of tungsten oxide
etch of tungsten oxide
2003-05-21
Allen Chou
2003-05-22
Justin Borski
2003-05-22
[email protected]
etch of tungsten oxide
Justin Borski
2003-05-22
You might try a 5% HCL dip for 30 seconds.

Justin C. Borski
MEMS Program Manager
Advanced MicroSensors Inc.
[email protected]
www.advancedmicrosensors.com



-----Original Message-----
From: Allen Chou [mailto:[email protected]]
Sent: Wednesday, May 21, 2003 7:11 PM
To: [email protected]
Subject: [mems-talk] etch of tungsten oxide


Hi,

Does any one know any chemical that can remove the
oxidized surface tungsten film without appreciable
damage on the tungsten?

Thanks,

Allen

__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.
Addison Engineering