Hi Mahdu,

Try dilute HF (1: 40). On the wafers that I have, there are NiFe structures,
I etch 200 Angstrom of Titanium around these structures and the NiFe is not
affected by the etch (around 20 seconds)

Best of luck

Magali

--
Energy Processing for ICT
NMRC, Lee Maltings, Cork, Ireland

Tel: +353 (0)21 4 904279
Fax: +353 (0)21 4 270271

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of madhulika sathe
Sent: 23 May 2003 17:42
To: [email protected]
Subject: [mems-talk] Titanium etch



I am looking for an etch for Titanium that does not affect the following:

1:Nickel
2:Iron

Any help in this regard would be greatly appreciated.

Thanks in advance!

Madhu
LSU



Need a new email address that people can remember
Check out the new EudoraMail at
http://www.eudoramail.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review