Titanium etch
2003-05-23
madhulika sathe
2003-05-27
Magali Brunet
2003-05-27
[email protected]
Titanium etch
[email protected]
2003-05-27
Hi Madhu

I use 10:1 BOE (Buffered Oxide etch) to etch Titanium, the
etch rate for sputtered Ti is 11kA/min. I use evaporated Ti
& my etch rate is roughly half of that.

I do not have information for Fe & Nickel, but since 10:1
BOE is fairly commonly available in most labs you might want
to determine the etch rates. Overall 10:1 BOE gives me good
& uniform results for Ti etching

Good Luck

Anupama




> I am looking for an etch for Titanium that does not affect
> the following:
>
> 1:Nickel
> 2:Iron
>
> Any help in this regard would be greatly appreciated.
>
> Thanks in advance!
>
> Madhu
> LSU
>
>
>
> Need a new email address that people can remember
> Check out the new EudoraMail at
> http://www.eudoramail.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or
> change your list options, visit
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing
> services. Visit us at http://www.memsnet.org/

Anupama V. Govindarajan
Graduate Student - EE MEMS laboratory
Department of Electrical Engineering
University of Washington
Campus Box 352500, Seattle WA 98195
Phone: (206)-221-5340
email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
MEMS Technology Review
Tanner EDA by Mentor Graphics