PDMS by SEM
Paul Monaghan
2003-06-03
Pan,

score the backside of your PDMS device perpendicular to the channel with a
sharp scalpel blade (not all the way through otherwise you will have scalpel
cutting marks) then gently bend over to split at the score mark - you should
get a nice clean cut without scalpel marks at your area of interest to SEM -
you have to be careful when coating with gold for SEMs, the gold often
flakes off due to the flexible of PDMS

hope this helps,

Paul

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Pan Mao
Sent: 03 June 2003 04:41
To: [email protected]
Subject: [mems-talk] PDMS by SEM


Dear all,

I have made the PDMS microfluidic channel and want to see the cross-
section of the channel by using SEM. However, it seems that I need to cut
a very shrap surface of my interest. Is it required? I would like to know
if any one has some experience on it. Your suggestions will be greatly
appreciated.

Thanks a lot,

Pan Mao

________________
USTC Alumni Email System, http://mail.ustc.edu,  FREE Signup.

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics