MEMSnet Home: MEMS-Talk: RIE process parameters for Si Etching
RIE process parameters for Si Etching
2003-06-11
Priyank Gupta
2003-06-12
ShuTing Hsu
2003-06-12
[email protected]
2003-06-13
Blunier, Stefan
RIE process parameters for Si Etching
Priyank Gupta
2003-06-11

hi!,
I have some problem with etching of silicon using RIE process. I'm wodering if
anyone knows about the process parameter (about 1-2 micrometer), gas used,
photresist, pressure, rf power etc. for etching of Si.

Thanks
Priyank Gupta
Research Assistant
ECEN
Oklahoma State University

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.
MEMS Technology Review