RIE process parameters for Si Etching
ShuTing Hsu
2003-06-12
HI Priyank

What kind of etching do you plan to do?
Which chamber? If you give me your baseline recipe and tell me what was
wrong,
Maybe I can help you tune the recipe in.

ShuTing
Electrical Engineering, UCLA


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Priyank Gupta
Sent: Wednesday, June 11, 2003 4:15 PM
To: [email protected]
Subject: [mems-talk] RIE process parameters for Si Etching




hi!,
I have some problem with etching of silicon using RIE process. I'm
wodering if
anyone knows about the process parameter (about 1-2 micrometer), gas
used,
photresist, pressure, rf power etc. for etching of Si.

Thanks
Priyank Gupta
Research Assistant
ECEN
Oklahoma State University

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.