Anodic Bonding
Tomblin, Graham (OH32)
2003-06-23
Try TWI ( the welding institute in London)also try searching for "mallory bond"
and Field assist bonding ref sensors and materials, 3 (1988) 143-151, key words
field -assisted bonding,FAB, interfacial
strength,fracture limit, micromechanics
-----Original Message-----
From: mems greenhorn [mailto:[email protected]]
Sent: Tuesday, June 17, 2003 7:34 PM
To: [email protected]
Subject: [mems-talk] Anodic Bonding


Can anyone let me know where I can find a good paper on Anodic Bonding..Trying
to do the anodic bonding at device level
for the first time..so need info on the procedure involved ...
- Are there any restrictions on the type of  Oxidation ( Thermal or PECVD)  that
Si wafer should have..
- What wafer thickness and oxide thickness would be ideal. ?
- What voltage and temperatures ?
- Significance of the mechanical pressure...?
- Is vaccum a must ?
Any other info that u can give to get a good bonding would be of great help !
Thanks in advance.
MEMS_GREENHORN


---------------------------------
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.