2003-06-23
Hi Srinivas

   You can go to websites of other universities to find out a typical recipe
for SI3N4.  You can try out Berkeley's Si3N4 etch using LAM Auto etcher.

argon.eecs.berkeley.edu

Phil Tabada



>From: "Srinivas Parimi" 
>Reply-To: General MEMS discussion 
>To: 
>Subject: [mems-talk] RIE of Si3N4
>Date: Sun, 22 Jun 2003 22:32:43 -0500
>
>Hello all,
>
>I would like to know if there is a standard RIE recipe to etch Si3N4
>selectively over Si and the etch rate of the process and the
>selectivity.
>
>
>Thanks in advance,
>
>Srinivas Parimi
>Research Assistant
>Center for Microelectronic Sensors and MEMS (CMSM)
>372 ERC
>University of Cincinnati
>Cincinnati OH 45221
>(513) 556 4795
>[email protected]
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Add photos to your messages with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation
University Wafer