[email protected]
2003-06-25
transene
Photoresist for AU plating
transene
2003-06-25
Transene Company offers a sulfite gold plating solution, TSG-250, with
better photoresist compatibility than cyanide solutions.  Information
may be found at www.transene.com.

Christopher Christuk
Transene Company

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Tuesday, June 24, 2003 4:03 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Photoresist for AU plating

I think ur gold bath is sightly alkaline, isn't it?
Alkaline will dissolve positive photoresists. I think you
might try negative photoresists instead since negative
photoresists doesn't dissovle in alkakine.

> Hi all,
>
> I was doing gold electroplating using cynide bath.I
> was doing plating on Si wafer sputtered with gold
> later covered with photoresist ,exposed and developed
> and hardbaked.
>
> after doing the above i have tried AU electroplating.I
> was  going for very low current densities and very low
> temperature and with optimum PH after very less time i
> could obsevere the plating of gold but the Photoresist
> is disturbed and the pattern was disturbed.
>
> Can i find any ways to improve adhesion of photoresist
> on AU surface.
>
> Ur suggestions are highly appreciated.
>
> Thanks
> Kris
>
>
> __________________________________
> Do you Yahoo!?
> The New Yahoo! Search - Faster. Easier. Bingo.
> http://search.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or
> change your list options, visit
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing
> services. Visit us at http://www.memsnet.org/

Best Regards,
Kin




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics