Ti Etch
2003-07-02
[email protected]
Ti Etch
[email protected]
2003-07-02
Try H2O2 at 40oC-50oC. It takes arround 0.5-1 hour to etch.
It will not attack Al.

>
> Dear all,
>
> I am trying to etch Ti(300 Angs),which has aluminum
> layer underneath it.I have used TiW-30 (25-40C)from
> transene.I could see that after some time the Ti etch
> rate reduces completely and etch almost stops.I think
> due to the formation of Tio2 the etch rate drops.
>
> Can anyone suggest me a good Titanium etchant that
> should not attack Al.
>
> Your suggestions are highly helpful.
> Thanks
> Kris
>
> __________________________________
> Do you Yahoo!?
> SBC Yahoo! DSL - Now only $29.95 per month!
> http://sbc.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or
> change your list options, visit
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing
> services. Visit us at http://www.memsnet.org/

Best Regards,
Kin


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
MEMS Technology Review