MEMSnet Home: MEMS-Talk: Cu Metal Etchant
Cu Metal Etchant
2003-07-02
이태원
2003-07-02
Greg Reimann
Making holes in Pyrex glass wafers?
2003-07-03
Gautham Viswanadam
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
Bill Flounders
2003-07-09
Carsten Wesselkamp
2003-07-03
David Nemeth
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-02
Pavel Neuzil
2003-07-03
Lin, Yaojian
Cu Metal Etchant
이태원
2003-07-02
hi.

I heard about Cu could be patterned by something like CMP Process ( damascene(?)
process)

Are there any wet etchants fot Cu etch? If not, what is the main reason about
that?

Furthermore, Adhesion layer (Ti or Cr) is not required when I deposit Cu on Si
Wafer ?

Thank you for in Advance.

TW Lee.

-----------------------------------------------------------
AeroMEMS Laboratory.
School of Mechanical & Aerospace Engineering.
Seoul National University , Seoul , KOREA.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
University Wafer
Addison Engineering