A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Cu Metal Etchant
Cu Metal Etchant
2003-07-02
이태원
2003-07-02
Greg Reimann
Making holes in Pyrex glass wafers?
2003-07-03
Gautham Viswanadam
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
Bill Flounders
2003-07-09
Carsten Wesselkamp
2003-07-03
David Nemeth
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-02
Pavel Neuzil
2003-07-03
Lin, Yaojian
Cu Metal Etchant
Greg Reimann
2003-07-02
DA Nanomaterials sells a CMP slurry for copper.  Don't know how you
would use it to pattern anything though.

Transene sells etchants for just about everything including copper.

You will need an adhesion layer especially if you are going to polish
it.  Ti is working better for me than chrome, but I am trying to get
them both to work.

Greg Reimann
Boston University

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of ÀÌÅ¿ø
Sent: Wednesday, July 02, 2003 11:01 AM
To: [email protected]
Subject: [mems-talk] Cu Metal Etchant

hi.

I heard about Cu could be patterned by something like CMP Process (
damascene(?) process)

Are there any wet etchants fot Cu etch? If not, what is the main reason
about that?

Furthermore, Adhesion layer (Ti or Cr) is not required when I deposit Cu
on Si Wafer ?

Thank you for in Advance.

TW Lee.

-----------------------------------------------------------
AeroMEMS Laboratory.
School of Mechanical & Aerospace Engineering.
Seoul National University , Seoul , KOREA.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Nano-Master, Inc.
Mentor Graphics Corporation