DSP vs SSP
2003-07-02
Tom Fan
2003-07-03
beaton@npphotonics (Bill Eaton)
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
Brubaker Chad
DSP vs SSP
Kirt & Erika Zipf-Williams
2003-07-03
> Wafers have two polishing options: Double Side Polished or Single Side
> Polished. I am wondering whats the particular applications for these two
types
> of wafers? Why are they differentiated?
> Anybody could enlighten me?

If you need to do lithography or wafer bonding on the back side of the wafer
(as is required for many MEM devices),
DSP is needed.
    --Kirt Williams, Ph.D.    consultant


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review