MEMSnet Home: MEMS-Talk: Poly polishing slurry
Poly polishing slurry
2003-07-04
Kumar Soma
2003-07-07
Michaela Wullinger
Poly polishing slurry
Kumar Soma
2003-07-04
Dear all,

I am looking for different types of slurry that can be used to polish poly. Also
any suggestion on type of pad and recipe are greatly appreciated. Any
information of surface roughness related to it will be highly beneficial. Many
thanks.

Kumar



---------------------------------