MEMSnet Home: MEMS-Talk: Making holes in Pyrex glass wafers?
Cu Metal Etchant
2003-07-02
이태원
2003-07-02
Greg Reimann
Making holes in Pyrex glass wafers?
2003-07-03
Gautham Viswanadam
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
Bill Flounders
2003-07-09
Carsten Wesselkamp
2003-07-03
David Nemeth
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-02
Pavel Neuzil
2003-07-03
Lin, Yaojian
Making holes in Pyrex glass wafers?
Bill Flounders
2003-07-07
Alternate Ultrasonic Machining Contact:
Perhaps related?

J.A. Anderson Associates
Precision Glass/Ceramics and Ultrasonic Machining
630-377-6565
[email protected]
www.jaanderson.com

Bill Flounders, Ph.D.
Technology Manager
Berkeley Microlab




Kirt & Erika Zipf-Williams wrote:
>>Hi, We are looking for supplier who can drill more than 1 mm holes on
>
> thick
>
>>(1 mm) Pyrex glass wafers. Please write to [email protected] Regards.
>
>
> Check with Sensor Prep Services in Illinois at 630-365-9645.
> They do ultrasonic drilling through even thicker glass.
>
>     --Kirt Williams, Ph.D.   consultant
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics