A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: platinum on SU-8
platinum on SU-8
2003-07-01
Chen-Han Lee
2003-07-03
Kirt & Erika Zipf-Williams
2003-07-07
sokwon Paik
2003-07-07
Chen-Han Lee
2003-07-07
Mighty Platypus
2003-07-09
Chen-Han Lee
2003-07-07
Kirt & Erika Zipf-Williams
2003-07-01
[email protected]
2003-07-08
[email protected]
platinum on SU-8
sokwon Paik
2003-07-07
I do not recommend evaporation method.
As platinum melting temperature is very high and vapor
pressure is very low even at Au melting temperature,
SU-8 layer could be easily burned by high temperature
of evaporator temperature.
Try sputtering.

Regards,

Sokwon Paik

--- Kirt & Erika Zipf-Williams
 wrote:
> > Good day everyone,
> > I am a research student in U.K.
> > Could anyone please tell me wome ways i can
> deposite platinum film on
> SU-8?
> > Any suggestions are welcomed.
> > Thank you for your time.
> > Chen-Han Lee


__________________________________
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
http://sbc.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing