MEMSnet Home: MEMS-Talk: RE: MEMS material
RE: MEMS material
2003-07-07
Jonathan Engel
RE: MEMS material
Jonathan Engel
2003-07-07
Kevin-

Nichrome (nickel chrome, 80/20) alloy fits most of your requirements.  It has
high resistivity (~100 uOhm*cm), a modulus of ~200 Gpa, yield strength ~450
Mpa, and a CTE of ~15e-6/C.  Deposition is usually performed via e-beam
evaporation or sputtering which are relatively low temp (<600C).  There are
likely other choices as well.  Good luck.

-Jonathan Engel
MASS Group, UIUC
http://mass.micro.uiuc.edu

>----- Forwarded Message -----
>From: General MEMS discussion 
>To: MEMS Talk 
>Subject: [mems-talk] MEMS Material !!
>
>Hello,
>I am looking for a  material for MEMS Actuators .
>I need a high eough resitivity material for Joul Heating purpose and a
resonable yiled strenth ( > 500 Mpa) .
>It's Young's modules *Coefficient of Thermal Expansion must be great than
polysilicon's. ( > 170Gpa*2.9e-6).
>Last of all, the dopositing temperature has to be lower than 600 degree and
the thinnest layer need to be deposited would be 500nm.
>Are there any thin film materials like this???
>
>Thanks in Advance!!
>
>Regards,
>Kevin YU


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics