Michaela Wullinger
Re: AW: [mems-talk] Protect backside of Si wafer from TMAH
2003-07-08
nga
Protection of backside of chips in TMAH
2003-07-10
kris
2003-07-11
Oray Orkun Cellek
2003-07-11
transene
2003-07-07
Roger Shile
2003-07-07
Mario Robles
Protect backside of Si wafer from TMAH
Mario Robles
2003-07-07
Hello,

You can try contacting Furukawa Electric in Tokyo, Japan. I believe they
have a UV tape that is used to protect the front side of a patterned
wafer during an etching process.

I believe this is their phone number, 3-3286-3213

Thank you,

Mario Robles

Tanaka Systems, Inc.
2577 Leghorn Street
Mountain View, CA 94043

650-966-8001 ofc
650-966-1881 fax
www.dicingblades.com


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Pimpin Alongkorn
Sent: Saturday, July 05, 2003 10:31 PM
To: [email protected]
Subject: [mems-talk] Protect backside of Si wafer from TMAH

Dear Folk,

I would like to purchase a wafer holder for wet etching that can protect
a
backside of wafer from etchant solution such as HF, TMAH and KOH. Could
you
recommend me a Japan company (or other countries are O.K.)? It will be
invaluable help for me. Thank you very much.

Alongkorn Pimpin
THT laboratory

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
The Branford Group
Harrick Plasma, Inc.