A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: V-grooves
sputtered silicon oxide
2003-07-09
Torsten Kießling
2003-07-09
PRAMOD GUPTA
Micro Chip Solutions
2003-07-10
Absara Micro Ststems
Re: V-grooves
2003-07-10
Romana Maryla Krolikowska
2003-07-10
Roger Shile
2003-07-10
beaton@npphotonics (Bill Eaton)
2003-07-11
Absara Micro Ststems
2003-07-12
weiwei2
Re: V-grooves
Roger Shile
2003-07-10
If you're using a crystallographic etch, such as KOH, edges of the grooves
will be stepped of they aren't aligned with the <110> planes of the Si.

I have seen residue after KOH etching Si which appears which appears as
submicron globs on a SEM, though I can't see it on an optical microscope.
This particular contamination is easily removed with Piranha.  I am curious
to know what it is.

Roger Shile

----- Original Message -----
From: "Romana Maryla Krolikowska" 
To: 
Sent: Thursday, July 10, 2003 5:18 AM
Subject: [mems-talk] Re: V-grooves


> I  am trying to etch V-grooves in 100 Silicon wafers. I use a silicon
> nitrate as a protective layer (approx. 50nm). I use a perspex beaker and
> teflon holder. I am  having  a few problems with the process.
> 1. the side walls of my V-grooves show often waviness
> 2. the walls are often contaminated with small particles (in the form of
> whitish grains) which are difficult to remove. (I use an acid bath to
> remove it).
> Could anyone help and suggest some solutions?
>
> Thanks in advance
>
> Maryla
>
> Laser Physics Centre,
> Ausralian National University
> Canberra
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation