MEMSnet Home: MEMS-Talk: Protection of backside of chips in TMAH
Protect backside of Si wafer from TMAH
2003-07-06
Pimpin Alongkorn
2003-07-07
Bill Flounders
2003-07-08
Michaela Wullinger
Re: AW: [mems-talk] Protect backside of Si wafer from TMAH
2003-07-08
nga
Protection of backside of chips in TMAH
2003-07-10
kris
2003-07-11
Oray Orkun Cellek
2003-07-11
transene
2003-07-07
Roger Shile
2003-07-07
Mario Robles
Protection of backside of chips in TMAH
Oray Orkun Cellek
2003-07-11
Dear Kris,

You may try to put a droplet of photoresist on a silicon wafer or glass,
stick your sample onto it, and do a soft bake.  After the etching, acetone
immersion will release your sample.  I guess this will not change the PH.

Best regards,

Oray Orkun Cellek
Research Assistant, Ph. D. Student
Electrical & Electronics Engineering Department
Middle East Technical University
06531 Ankara
Turkey
Tel : +90 312 210 4579
Fax : +90 312 210 1261
e-mail : [email protected]

----- Original Message -----
From: "kris" 
To: "General MEMS discussion" 
Sent: Thursday, July 10, 2003 9:20 PM
Subject: [mems-talk] Protection of backside of chips in TMAH


> Dear all,
>
> I am trying to etch si in TMAH solution.I have very
> small chips(not wafer) to be etched.As we need to have
> mild stirring for the etchant solution,i was wondering
> how to place my chips in the etchant solution.
>
> Is there anyway that i can etch small chips in TMAH
> solution.I want to know if there is any vendor who can
> supply me epoxy so that i can attach my chips to any
> glass substrate and cure them which also protects the
> backside of the chips.I need epoxy that should not
> change PH of the solution as the etch process is
> highly sensitive to the change in PH values.
>
> Your suggestions would be highly grateful.
>
> Thanks
> Kris
>
> __________________________________
> Do you Yahoo!?
> SBC Yahoo! DSL - Now only $29.95 per month!
> http://sbc.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation