A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Protection of backside of chips in TMAH
Protect backside of Si wafer from TMAH
2003-07-06
Pimpin Alongkorn
2003-07-07
Bill Flounders
2003-07-08
Michaela Wullinger
Re: AW: [mems-talk] Protect backside of Si wafer from TMAH
2003-07-08
nga
Protection of backside of chips in TMAH
2003-07-10
kris
2003-07-11
Oray Orkun Cellek
2003-07-11
transene
2003-07-07
Roger Shile
2003-07-07
Mario Robles
Protection of backside of chips in TMAH
transene
2003-07-11
Kris,

Transene Company offers epoxy resins which would meet your needs.  We
also offer TMAH as well as proprietary isotropic and anisotropic silicon
etchants.  Our products may be viewed at www.transene.com.

Feel free to contact me if you would like to discuss your application
further.

Christopher Christuk
Transene Company
10 Electronics Avenue
Danvers MA  01923
Tel:  978 777 7860
Fax:  978 739 5640
Email:  [email protected]

-----Original Message-----
From: kris [mailto:[email protected]]
Sent: Thursday, July 10, 2003 2:21 PM
To: General MEMS discussion
Subject: [mems-talk] Protection of backside of chips in TMAH

Dear all,

I am trying to etch si in TMAH solution.I have very
small chips(not wafer) to be etched.As we need to have
mild stirring for the etchant solution,i was wondering
how to place my chips in the etchant solution.

Is there anyway that i can etch small chips in TMAH
solution.I want to know if there is any vendor who can
supply me epoxy so that i can attach my chips to any
glass substrate and cure them which also protects the
backside of the chips.I need epoxy that should not
change PH of the solution as the etch process is
highly sensitive to the change in PH values.

Your suggestions would be highly grateful.

Thanks
Kris

__________________________________
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
http://sbc.yahoo.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.