I've dug through the MEMS-talk archives trying to find out some info on wet
etching of Pyrex. Most of the posts address to deep glass etching and most
people use Cr/Au as etching masks. I want to do a shallow etch (4 um) instead.
Would photoresist be able to stand HF for such a shallow etch or Cr/Au still
need to be used? I also learned from the past discussion that photoresist does
not adhere well to Pyrex wafers. Is this true? This is the reason that Cr is
deposited before the photoresist, but what is the role of Au then?

Thanks,
Tom Fan


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group